I. Overview
By conversing electrics into thermal energy, the equipment is used to maintain the metal liquid in constant temperature (commonly known as holding machine or casting machine). It is widely applied to smelting, forging and casting. According to the properties of specific product, isothermal casting can be conducted in the specified smelting temperature, so as to guarantee the product quality; it can be used in fixed-point or unfixed-point casting; it can also be used in continuous or intermittent casting; it is especially suitable to the production operation of casting line, for its advantages in greatly fastening casting speed and improving the quality of forging product and etc.
II. Configuration
Furnace framework (flat car) 1 pc/ set
Furnace body 1 set
Furnace lid 1 pc
Operating device 1 set
Power supply control cabinet 1 set
Ground rack 1 set
1:72 reducer 3 pcs
III. Technical Parameters
1. Specification of power (300kw)
A、1t: B、1.2t : C、1.5t:
2. Input voltage 400v Output voltage 800v working voltage frequency 500hz
3. Displacement distance of the whole machine X direction 3~4.m Z direction 1.4m
4. Casting height (distance from sprue to the mould-filling box): 60~200mm (in Y direction)
IV. Operating Instructions:
1. For furnace repair, it is feasible to refer to intermediate-frequency furnace; after repair, the furnace shall be baked to dry by ladle dryer;
2. Prepare relevant auxiliary facilities and tools for casting in advance, such as buffer pallet; conduct routine pre-booting check: whether the lubrication, operation and the power supply are normal; clamp the plug rod in place;
3. Start up the water-cooling circulation system, turn on the power supply, and the iron liquid flows into the constant-temperature furnace from tundish. Then cover the furnace lid and start up and heat the furnace to the setting temperature;
4. Adjust the flat car to align the sprue with the mould-filling box and then commission the pull rod to align the casting position until it is aligned to the correct place, and then carry out the normal casting;
5. After casting, lift away the furnace lid, and conduct water cooling over the furnace; when the temperature of furnace is cooled down to about 80℃, stop flushing and just let the furnace cool itself down.
6. Clean the furnace pit.
7. Keep water circulation running for 3 hours.
Next:Intermediate-frequency Melting Furnace |